img Accessibility Controls

Technologies Banner

All Technologies

Cold Bonded Carbon Composite Pellets for Utilization of Iron Ore Micro-Fines and Carbon Bearing Fines

Project Overview

This process produces micro-pellets with high C content which will be used in sintering of iron ore for reduction of coke breeze consumption and in smelting reduction process with a short curing time.

Benefits

This is a cold bonding process, so it is energy efficient. Curing time is very short (5-10 min), It utilizes iron ore micro-fines and coal fines or coke fines or carbon containing waste fines in iron making or sintering, The micro-pellets provide energy to the sinter bed for reduction in coke breeze consumption. 38-48 % reduction in coke breeze has been found when 38 % blast furnace flue dust containing pellets were mixed with iron ore in sintering (12 kg scale), Since it is a composite pellet, it can be reduced faster than normal pellets C02 in steel plant''s waste gas is utilized in strengthening of pellet.

Source

Quick Information
Thrust Areas
Chemical Sciences
Focus Area
Utilisation of Iron Ore
Source Title
Output
TRL: Technology Readiness Level
Technology Development
arrowtop
Latest Updates
Loading…